The Beta zeolite produced by means of a template agent based hydrothermal crystallization method is featured with high relative crystallinity,wherein the relative crystallinity is no less than 80%,the SiO2/Al2O3 molar ration is no less than 50,and the Na2O is no more than 0.1%,and the BET specific surface is no less than 500m2/g