DYM1can be absorbed on the surface of the cement slurry hydrate to inhibit contacting with water and chelating with Ca2+ to prevent crystal nucleus from forming early. Therefore ,it can retard thickening time.
Characteristics:
DYM1 consists of sulfonate and organic salts.
Appearance: Light yellow or brown powder
Normal dosage:0.7%-2.0%(BWOC)
Suitable temperature: 110℃~170℃(BHCT)
Reduce consistency of cement slurry and improve the rheology
The thickening time is adjustable
Has no harmful influence on other properties of cement slurry
Technical specification:
Items |
Specification |
Appearance |
Light yellow or brown powder |
Initial consistency Bc |
≤30 |
Thickening time,min/118℃,70MPa,60min |
180-240 adjustable |
Compression strength,Mpa/142℃,21Mpa,48h |
≥14 |
The ingredients of cement slurry in the table are:JiaHua G class cement 594g+silica sand :208g(160-200mesh) Distilled water 333ml DYM1:0.7-2.0%
Packing,storage:
Be sacked with three-layer plastics bag,25KG per bag