Film Grade HDPE
ItemTest conditionTest MethodValueUnitDensity-ISO 11830.944-0.955g/cm3MFR190°C/2.16kgISO 11330.03-0.07g/10minTensile strength at yield-ISO 527-222MPaElongation at break-ISO 527-2>350%ESCRF50,50°C,100%ASTM D-1693A1000hVICAT-ASTM D-1525126°C
Blowing molding Grade HDPE
ItemTest conditionTest MethodValueUnitDensity-ISO 11830.950~0.955g/cm3MFR190°C/2.16kgISO 11331.7~2.5g/10minTensile strength at yield-ISO 527-224MPaElongation at break-ISO 527-2>600%
Injection grade HDPE
ItemTest conditionTest MethodValueUnitDensity-ASTM D-7920.9545g/cm3MFR190°C/2.16kgASTM D-123820g/10minTensile strength at yield-ASTM D-63828MPaElongation at break-ASTM D-638250%Impact tensile strength-ASTM D-182242kJ/m2ESCR-ASTM D-16933-VACIT-ASTM D-1525127°C