Sodium Diethylhexyl Sulfosuccinate
-
- Category :
Other Chemicals
- CAS NO : 1639-66-3
- EC NO : 216-684-0
- Molecular Formula : C20H38O7S
- Main Specifications :
- Synonyms : Rapid Penetrant T;sodium 1,4-bis[(2-ethylhexyl)oxy]-1,4-dioxobutane-2-sulfonate;sodium 1,4-bis(octyloxy)-1,4-dioxobutane-2-sulfonate;1,4-bis(octyloxy)-1,4-dioxobutane-2-sulfonic acid;
Package: Package: 200L plastic drum, IBC(1000L),customers’ requirement.
Uses : (5) Usage in asbestos: for froth asbestos, the preferred dosage is 10-15% of asbestos; for dustless asbestos, the preferred dosage is 15-20% of asbestos. (6) Usage in tanning: for dry tanning, this product is usually mixed with jfc, and the preferred dos
Molecular Structure:

Product description:
Sodium Diethylhexyl Sulfosuccinate
Synonyms: Penetrant OT, Penetrating agent T CAS NO.: 1639-66-3
Molecular formula: C20H37NaO7S Molecular weight: 444.56
Structural Formula:
Properties:
This product is an anionic surfactant, it has properties of rapid penetration, homogeneity, wetting, emulsification and better frothing. It is intolerant with strong acid, strong alkali, heavy metals and reductant.
This product is soluble in water, lower alcohol, benzene, ccl4 and kerosene oil solvents. The solution is milk white, pH (1% water solution) is 5.0-7.0.
This product can penetrate rapidly and homogeneously, and has good effect at temperature lower than 40℃ and pH 5-10. The treated fabric is stable even temperature acidic and alklic condition changed. It’s widely used textile & dyeing, pesticide emulsification, tanning and mineral separation.
Specification:
Items Index
Appearance Colorless to yellow viscous liquid
pH (1% water solution) 5.0-7.0
Penetrating (1% water solution) /s 5.0 max
Solid content % 50.0 min
Methods and used in
(1) Cotton wool dyeing: 2g/l of this product is heated from room temperature to 95℃, 20 min dehydration, then rolling drift after cooling, cleaning, dechloridation.
(2) Cotton wool lian drift: cotton wool is pretreated at 20℃ for 5 min, then other additives can be added, it is heated to 80-90℃ in 20-30 min, and is treated for 45 min. When cotton shell is removed, it can be dyed. The preferred dosage is 2-3g/l.
(3) Cotton wool lian, drift and dyeing: The direct or active dye which is oxidant tolerance is selected. The method is the same as 2, dyeing is added directly.
(4) Scouring of adhesive: addition of penetrant t in scouring of adhesive can reduce 2 h and decrease damage to silk.
(5) Usage in asbestos: for froth asbestos, the preferred dosage is 10-15% of asbestos; for dustless asbestos, the preferred dosage is 15-20% of asbestos.
(6) Usage in tanning: for dry tanning, this product is usually mixed with jfc, and the preferred dosage is 0.5-1.0%. For tanning additives, the preferred dosage is 10%.